How to Weld Type 2205 CodePlus Two®Duplex Stainless Steel

Material Description

2205 is a duplex (austenitic-ferritic) stainless steel thatcombines many of the best properties of austeniticand ferritic stainless steels. High chromiumandmolybdenum contents provide excellent resistanceto pitting and crevice corrosion. The duplexstructureis highly resistant to chloride stress corrosioncracking. 2205 has outstanding strength andtoughness and possesses good weldability.

The trademark Code Plus Two®indicates thecommitment, not only to meet the requirementsfor S31803 as established in ASTM and ASME,but also to meet two additional requirements. The first requirement was that nitrogen should bein the 0.14 to 0.20% range to gain its benefits inhigher strength, higher corrosion resistance, greatermetallurgical stability, and superior propertiesafter welding. The second requirement was thatall mill products should pass a test for the absenceof detrimental intermetallic phases. The tests

developedby Outokumpu Stainless for this purposehave been formalized as the ASTM A 923 standardtest method.

Specifications

UNS S32205, S31803 (wrought products)UNS S39209 (bare welding wire)UNS J92205 (cast products)Plate, Sheet, StripBar, BilletPipe, TubingForgings, FittingsCastingsTesting

ASTM

A 240, A 480A 276, A 479

A 789, A 790, A 928A 182, A 815A 890A 923

ASME

SA-240, SA-480SA-479

SA-789, SA-790SA-182, SA-815

These special requirements now define a newquality of 2205, designated S32205. S32205 isdual certifiable as S31803, but represents whatusers have come to expect of 2205 steel. BothS31803 and S32205 are included in all applicableASTM product specifications.

The increased strength of S32205, relative tothat of S31803, resulting from its higher nitrogen isnow being recognized by ASTM and ASME. TheASTM has designated S32205 as 2205.

Forming, Heat Treatment, and MachiningHot Forming

2205 is hot formed in the range 2250–1750°F(1230–955°C). In this range, the material has lowmechanical strength and good hot ductility. If slowcooled or held at temperatures between 600 and1750°F (315–955°C), the combination of strainand temperature can lead to rapid room temperatureembrittlement by the formation of sigma phaseand other detrimental intermetallic compounds.Full annealing with rapid cooling, ideally waterquenching, is recommended after hot forming.

Cold Forming

ASME Code Case 2186 (Embossed Assemblies)ASME/ANSI B16.34 for A 182, A 240, A 479, A 789, A 790ASME/ANSIB16.5, ASME/ANSI B31.1 Code Case 153ASME/SFA 5.4, SFA 5.9, and SFA 5.22 P No. 10H, Group 1AWS/A5.4 E 2209-XX, A5.9 ER 2209, A5.22 E 2209T0-XNACE MR0175

Because of its higher strength, 2205 requires higherforces for cold forming than those typical foraustenitic stainless steels. Additional allowance forspringback is necessary. Outokumpu Stainless 2205may be formed on equipment typically used forforming austenitic stainless steels, once allowancehas been made for its higher strength. Designs with2205 frequently have used its higher strength topermit reductions of gauge, significantly easingmany forming applications. Full annealing and

quenching is recommended after severe cold forming.

Heat Treatment

2205 is annealed at 1900°F (1040°C) minimumwith subsequent rapid cooling, ideally water