ADVANCED WIRE BONDING-BONDING ON COPPER

copper wire introduction

3. Oxidation of Copper Pad Surface

As oxidation of copper bond pad is the main issue, this is being looked into when it is still a wafer.

3.1 Wafer Dicing Process

Singulation of dice from a wafer is carried out by wafer dicing process. This involves sawing the wafer with a saw blade. As sawing process would generate high temperature, DI water is sprayed onto the cutting parts for cooling purposes. The submersion of entire wafer under DI water would readily oxidizes the copper bond pad during the dicing process.

Oxidation of the copper pad surface begins when the copper is exposed to the atmosphere. The copper oxides grows readily. Wafer dicing process not only oxidize the copper pad surface, it also introduce foreign particles such as silicon dust onto the surface. Figures 2a and 2b show pictures of the copper bond pad which were before and after dicing. It can be seen that there are some tiny particles around the bond pad after the dicing. These particles are suspected to be silicon dust. Comparing the copper bond pad to a normal aluminum bond pad, there are no such particles that are observed, see Figure 2c.

Figure 2a. Cu bond pad before dicing

Figure 2b. Cu bond pad after dicing

Figure 2c. Al bond pad after dicing

- 2 -

3.2 Die Attach and Adhesive Curing Processes

To attach the die onto the substrate, the die is picked and placed onto the substrate with adhesive material in between. The adhesive material is then cured in oven to achieve the mechanical properties. Depending on the type of adhesive materials used, the curing temperature range from 130 C to 180 C and curing time range from 1 minute to 90 minutes. The exposure of the die under this temperature would readily oxidizes the copper bond pad during the adhesive curing process.

In using a copper wafer, it is very important to select the type of die attach adhesive. Conventional die attach adhesives are not suitable for the copper wafer. This is because the typical curing time of this type of die attach is 30 minutes to 2 hours at a temperature of 150 C. It has to be noted that the oven used for copper wafer die attach curing needs to be either vacuum oven or filled with nitrogen gas. Figure 3a shows copper bond pads that have been oxidized after 30 minutes of curing at 150 C. The left bond pad shows a clear marking of non-stick ball contact area when gold ball bonding is carried out. Figure 3b is a typical aluminum bond pad after the same curing process. It can be seen that it is ”cleaner” when compared to the copper bond pad. As such it is preferred to use a snap cured die attach adhesive which has a curing time of 5 minutes at a temperature of 150 C. Figure 3c shows the copper bond pad surface after die attaching curing process with snap cured die attached adhesive. Under an optical microscope, the colour of the bond pad is brighter when compared to bond pad that has subjected to 30 minutes of curing at 150 C. It is therefore very important to note that snap cure oven have the advantage of avoiding excessive oxidation of copper bond pad during die attach curing process. In short, from view of copper pad oxidation, it is best to have the die attach curing process at the lowest possible temperature and shortness possible time.

Figure 3a. Oxidation of Cu bond pad after die attach

curing

Figure 3b. Al bond pad after die attached curing

ADVANCED WIRE BONDING-BONDING ON COPPER

ADVANCED WIRE BONDING-BONDING ON COPPER

ADVANCED WIRE BONDING-BONDING ON COPPER

ADVANCED WIRE BONDING-BONDING ON COPPER

ADVANCED WIRE BONDING-BONDING ON COPPER

process

上一页第2页

你可能喜欢

热门文档

相关文档

  • Copper_Wire_Bonding_Training

    Copper Wire Bonding Training 铜线焊线培训 Prepared by: Ning wy Shenzhen STS Microeletronics Copper Wire Bonding Content of Presentation 内容介绍 Advantages优点...

  • Developments in Copper Wire Bonding

    Drivers for Cu Wire Bonding ? ? ? ? Cost, cost and cost Gold price continues to increase: $1,515.17/oz on 2011-05-04 Copper: $4.15/lb Early...

  • Fine Pitch Copper Wire Bonding Process and Material...

    Wire Bonding Optimizatio... 6页 20财富值 Gold Wire Bonding On Low... ...The study has shown the utilization of advanced wire bonder copper capability...

  • Wire bonding workmanship standard

    wire bonding工艺文件 12页 2下载券 Copper Wire Bonding 5页 7下载券 喜欢...REJECT if no gold ball and or wire observed on bond pad and substrate ...

  • Heraeus Copper Wire Presentation

    Market Review Challenges in Copper Wire bonding Heraeus Copper Wire Portfolio ...? Soft wire characteristics enable: ? Bonding on challenging pad structure. ...

  • Reliability of copper wire bonding in humidity envi...

    In present paper, copper wire bonding on palladium finish and gold finish was studied to investigate the interface degradation during uHAST comparing with ...

  • Wire Bonding process

    Hardening: Advanced deformation, diffusion initiate Saturation: Bond finished ... Fine Pitch Copper Wire... 8页 免费 Wire Bonding Summary 25页 免费 ...

  • Chapter7_Reliability_Advanced_bonding_interconnecti...

    Development of Copper Wi... 6页 20财富值 ... Advanced Bonding Interconnection Technology (Chapter...Bonding styles – Al wire bonding on Cu pad, ...

  • Cu wire bonding

    (<=1.3mil) ~ 26% of the TAM Bonding Wire 18 Copper Wire Market Trend...Materials Characteristics of Soft Copper Wires Designed for Advanced Applications...

  • ...and Feasibility of Copper Wire bonding for Non-h...

    Many studies have been done on copper wire bonding for equipment capability,...Also, an advanced tip surface finishing in order to executes better gripping...