EXPERIMENTAL EVALUATION OF MAN-MADE FIBRE BRITTLENESS
EXPERIMENTAL EVALUATION OF MAN-MADE FIBRE BRITTLENESS K. E. Perepelkin, N. V. Klyuchnikova, and N. A. Kulikova UDC 677.4.017.445
In the preparation, processing, and use of articles made from man-made fibres, one often encounters failure due to fibre brittleness, which leads to formation of a nap and dust, breakage, and also to a drop in the service properties of the articles. This is particularly marked in articles based on fibres with a high glass point: aramides, carbon fibres, silicates, and others. However, up until now brittleness has been one of the least studied mechanical properties of fibres and yarns; moreover, there has not been a clear definition of the concept of fibre brittleness, and this has hindered objective evaluation of this property. Failure of polymeric materials as a result of crack penetration which takes place in the elastic deformation region and is not accompanied by elastic deformation[i]. Brittle failure of polymeric materials, including fibres, takes place at a brittleness temperature (Tbr) which is considerably below the glass point, where even forced elastic deformation completely disappears. The brittleness temperature depends not only on the form of deformation (bending, stretching, compression), but also on the test method, particularly on the deformation rate[i] (the higher the rate of deformation, the higher Tbr is). At present, the Tbr of films and plastics is determined from the character of failure of a sample in bending under an assigned regime of rates and deformations[2, 3]; however, a similar determination of Tbr for fibres has proved to be impossible. To characterize the brittleness of fibres and yarns, methods are used which are based on analysis of the features of deformation in various forms of loading. In extension, brittleness is characterized by obedience of the stretching diagram to Hook's law up to the point of breakage. In bending, the critical radius of fibre bending serves as the brittleness index[4, 5]. The magnitude of strength loss on testing fibres in a knot is used for indirect evaluation of brittleness[6]Analysis of literature sources which throw light on questions of man-made fibre processing showed that a regime of joint action of bending and stretching is basic for fibres and yarns. However, fibre brittleness as applicable to these conditions has not been examined. In connection with the foregoing, in the present article we discuss the character of failure and evaluation of fibre brittleness under conditions of the joint action of bending and stretching. As objects of study we chose flexible-chain (polyacrylonitrile --PAN), stiff-chain (Terlon), carbon fibres (CF), and glass fibres, which have the following characteristics: Fibre PAN Teflon CF Glass Diameter, 12.0 9.0 7.4 9.5 Destructive tension, GPa 0.8 6.6 4.4 8.0 Modulus of deformation, GPa 4 I00 150 70
These fibres have various degrees of anisotropy in structure and properties, which fall off in the following order[7-9]:
Terlon, PAN, CF, glass. Moreover, they display various characters of failure. PAN fibres have an irregular form of failure surface; in failure, Terion partially fibrillates; and CF and glass fibres fail with a transverse penetration of cracks. The glass points of these fibres are also considerably different[7]: PAN, 75-90°C; Terlon, 345-380°C; CF, 1500-2000°C; glass fibre, 300-400°C. Let us examine the action of forces and the stress distribution in a f i b r e in various forms of deformation (Fig. I). Stress distribution in a fibre in stretching is uniform over its cross-section (Fig. la); in pure bending, it is symmetrical relative to a neutral line which passes along the fibre axis (Fig. ib); in bending with stretching, the neutral line is displaced inside the bending zone, so that stretching stresses become predominant (Fig. ic). The stress distribution in this case for a fibre which is approximated by a round cross-section will obey the equation of[i0] Translated from Khimicheskie Volokna, No. 2, pp. 36-37, March-April, 1989. title submitted September 17, 1988. 0015-0541/89/2102-0145512.50~1989 Plenum Publishing Corporation Original ar-
145

The self-made man 13页 免费 喜欢此文档的还喜欢 15570324-Textile-Fibre.....The development of manmade fibers —The development of rayon For centuries ...
Man-made wonders of the world_英语学习_外语学习_教育专区。英语交际英语教材《环球英语》相关课件。教材有12个单元,这些课件和某个单元的内容相关,有助于英语...
www.elsevier.com/locate/compositesb Evaluation on...However, the intrinsic brittleness of epoxy matrix...2. Experimental work 2.1. Materials The epoxy ...
415-422 Evaluation of the Mechanical Properties of...A way to circumvent the brittleness of the ...2. EXPERIMENTAL PROCEDURES Composites were fabricated...
Evaluation of Haynes 242 alloy as SOFC ...Based on the experimental results, the potential ...difficult to fabricate because of their brittleness...
Made from Man-Made Organic-Base Fibers Test ...Brittleness Temperature of Plastic Sheeting by ...(Uniform Abrasion) Practice for Evaluation of ...
Assessment of Man-made and Natural Hazards in the Surroundings of Hydropower Projects under Cons_专业资料。维普资讯 http://www.cqvip.com JunlfMonanSineo ...
Evaluation of Haynes 242 alloy as SOFC ...Based on the experimental results, the potential ...difficult to fabricate because of their brittleness...
热门文档